GEOBOND 25 KG BAG

Geobond

GeoBond® is a natural Miocene Diatomaceous Clay consisting of Diatomite (45%)and montmorillonite (55%). After mining, it is further processed using an exclusive wood burning method to enhance its active properties. The resulting product is a grey odorless granular material which has a density of about 40 lbs per cubic foot.

25 KG

All-Natural and Safe

GeoBond® does not bind vitamins or minerals and contains safe levels of chemical elements. When assessed for its toxic equivalence factor using the World Health Organization scheme, GeoBond® tested negative for any dioxin and furan pollutants. GeoBond® is OMRI-listed (Organic Materials Review Institute) natural diatomaceous clay consisting of roughly 45% diatomite and 55% montmorillonite. Both substances are generally recognized as safe (GRAS) by the FDA under CFR 573.340 and 581.1 respectively.

Better than Bentonite

GeoBond® has been proven to be more effective solution than sodium bentonite; GeoBond® has a bipolar charge which allows it a broader spectrum approach when dealing with safe feed challenges. Since GeoBond® is non-swelling clay it does not bind vitamins and minerals. GeoBond® also is very cost effective when comparing it to bentonite.

GeoBond® Versus Bentonite

GeoBond® Bentonite
Absorbent X X
Swelling X
Binds Vitamins X
Binds Minerals X
Polar Charge X
Bipolar Charge X
Pelleting Aid X
Multiple Binder X
Single Binder X

Analysis

Trace mineral chemical analysis by the Virginia Division of Mineral Resources.

Product Description: Clay fines from discharge

Method of Mineralogy Analysis: Product sample mixed with water, spread on x-ray slide, dried at 80 degrees C for 16 hours, and elemental chemistry determined with x-ray fractometer.

Mineralogy Analysis: Quartz/Illite

Method of Chemistry Analysis: Product sample mixed with water, spread on x-ray slide, dried at 80 degrees C for 16 hours, and elemental chemistry determined with x-ray fractometer.

Chemistry Analysis

MEAN % MEAN %
SiO2 75.29 Na2O 0.14
AI2O3 9.25 K2O 1.57
FeO3 2.90 TiO2 0.55
MgO 1.65 P2O5 0.45
CaO 1.86 LoI 6.33

geobond-omri

GeoBond® Is Pure And Safe

Maximum Tolerable Level
(ppm)
Level in treated feed at 2% inclusion
(ppm)
Cadmium .5 .06
Mercury 2 0
Selenium 2 0
Cobalt 10 .08
Molybdenum 10 .69
Vanadium 10 1.53
Barium 20 1.92
Tungsten 20 .03
Copper 25 .29
Lead 30 .26
Arsenic 50 .23
Nickel 50 .49
Iodine 50 .03
Antimony 70 .03
Boron 150 1.04
Aluminum 200 *
Bromine 200 1.53
Zinc 300 1.94
Bismuth 400 .01
Manganese 400 1.24
Chromium 1000 1.51

*Maximum tolerable level for aluminum refers to highly bioavailable soluble aluminum salts. The aluminum in GeoBond® is a natural and innocuous aluminum compound that is not highly bioavailable.

Better than Bentonite

GeoBond® has been proven to be more effective solution than sodium bentonite; GeoBond® has a bipolar charge which allows it a broader spectrum approach when dealing with safe feed challenges. Since GeoBond® is non-swelling clay it does not bind vitamins and minerals. GeoBond® also is very cost effective when comparing it to bentonite.

GeoBond® Versus Bentonite

GeoBond® Bentonite
Absorbent X X
Swelling X
Binds Vitamins X
Binds Minerals X
Polar Charge X
Bipolar Charge X
Pelleting Aid X
Multiple Binder X
Single Binder X

Analysis

Trace mineral chemical analysis by the Virginia Division of Mineral Resources.

Product Description: Clay fines from discharge

Method of Mineralogy Analysis: Product sample mixed with water, spread on x-ray slide, dried at 80 degrees C for 16 hours, and elemental chemistry determined with x-ray fractometer.

Mineralogy Analysis: Quartz/Illite

Method of Chemistry Analysis: Product sample mixed with water, spread on x-ray slide, dried at 80 degrees C for 16 hours, and elemental chemistry determined with x-ray fractometer.

Shipping & Returns

Pop-up link text View full details